不同浓度的丙二醇水溶液比重
来源于上海凯茵化工
更新于 2026.08.20
730
温度℃
丙二醇水溶液浓度(体积浓度)
10%
20%
30%
40%
50%
60%
70%
80%
90%
–35
1072.92
1079.67
1094.5
1092.46
–30
1071.31
1077.82
1090.85
1088.82
–25
1062.11
1069.58
1075.84
1087.18
1085.15
–20
1060.49
1067.72
1073.74
1083.49
1081.46
–15
1050.43
1058.73
1065.73
1071.51
1079.77
1077.74
–10
1039.42
1048.79
1056.85
1063.61
1069.16
1076.04
1074
-5
1027.24
1037.89
1047.02
1054.84
1061.37
1066.69
1072.27
1070.24
0
1013.85
1025.84
1036.24
1045.12
1052.71
1059
1064.09
1068.49
1066.46
5
1012.61
1024.32
1034.46
1043.09
1050.44
1056.5
1061.36
1064.68
1062.65
10
1011.24
1022.68
1032.55
1040.94
1048.04
1053.88
1058.51
1060.85
1058.82
15
1009.75
1020.91
1030.51
1038.65
1045.52
1051.13
1055.54
1057
1054.96
20
1008.13
1019.01
1028.35
1036.24
1042.87
1048.25
1052.44
1053.12
1051.09
25
1006.4
1016.99
1026.06
1033.7
1040.09
1045.24
1049.22
1049.22
1047.19
30
1004.54
1014.84
1023.64
1031.03
1037.18
1042.11
1045.87
1045.3
1043.26
35
1002.56
1012.56
1021.09
1028.23
1034.15
1038.85
1042.4
1041.35
1039.32
40
1000.46
1010.16
1018.42
1025.3
1030.98
1035.47
1038.81
1037.38
1035.35
45
998.23
1007.64
1015.62
1022.24
1027.69
1031.95
1035.09
1033.39
1031.35
50
995.88
1004.99
1012.69
1019.06
1024.27
1028.32
1031.25
1029.37
1027.34
55
993.41
1002.21
1009.63
1015.75
1020.72
1024.55
1027.28
1025.33
1023.3
60
990.82
999.31
1006.44
1012.3
1017.04
1020.66
1023.19
1021.27
1019.24
65
988.11
996.28
1003.13
1008.73
1013.23
1016.63
1018.97
1017.19
1015.15
70
985.27
993.12
999.69
1005.03
1009.3
1012.49
1014.63
1013.08
1011.04
75
982.31
989.85
996.12
1001.21
1005.24
1008.21
1010.16
1008.95
1006.91
80
979.23
986.44
992.42
997.25
1001.05
1003.81
1005.57
1004.79
1002.76
85
976.03
982.91
988.6
993.17
996.73
999.28
1000.86
1000.62
998.58
90
972.7
979.25
984.65
988.95
992.28
994.63
996.02
996.41
994.38
95
969.25
975.47
980.57
984.61
987.7
989.85
991.06
992.19
990.16
100
965.68
971.56
976.36
980.14
983
984.94
985.97
987.94
985.91
105
961.99
967.53
972.03
975.54
978.16
979.9
980.76
983.68
981.64
110
958.17
963.37
967.56
970.81
973.2
974.74
975.42
979.38
977.35
115
954.24
959.09
962.97
965.95
968.11
969.45
969.96
975.07
973.03
120
950.18
954.67
958.26
960.97
962.89
964.03
964.38
970.73
968.69
125
945.99
950.14
953.41
955.86
957.55
958.49
958.67
966.37
964.33