按语:本指南仅供参考。所有资料来源于一些技术性刊物,比较可靠,但由于实验影响因素众多,我们对此不作担保。望您在实际实验中先做预实验。中文名英文名尼龙膜ptfepvdf醋酸纤维膜硝基纤维素膜再生纤维素膜冰醋酸acetic,glacial●√√??√25%醋酸acetic,25%●√√●√√浓盐酸hydrochloric,concentrated??√??√25%盐酸hydrochloric,25%●√√√√√浓硫酸sulfuric,concentrated?√●??●25%硫酸sulfuric,25%?√√??√浓硝酸nitric,concentrated?√●???25%硝酸nitric,25%?√●●●√25%磷酸phosphoric,25%?√√√√√25%甲酸formic,25%?√√●√√10%三氯乙酸trichloroacetic,10%●√√√√√氢氧化铵ammoniumhydroxide,25%√√●√√○氢氧化钠sodiumhydroxide,3n√√√??○98%甲醇methanol,98%√√√√●√98%乙醇ethanol,98%√√√√●√70%乙醇ethanol,70%√√√√●√异丙醇isopropanol√√√√√√正丙醇n-propanol√√√√√√戊醇amylalcohol√√√??√丁醇butylalcohol√√√√√√苯甲醇benzylalcohol√√√●●√乙二醇ethyleneglycol√√√√●√丙二醇propyleneglycol√√√●●√甘油glycerol√√√√√√己烷hexane√√√√√√甲苯toluene√√√√√√苯benzene√√√√√√汽油gasoline√√√√√√氯甲烷methylenechloride●√√?●√氯仿chloroform●√√?√√三氯乙烷trichloroethane√√√?√√三氯乙烯trichloroethylene√√√√√√氯苯chlorobenzene(mono)√√√√√√四氯化碳carbontetrachloride√√?●√√丙酮acetone√√???√环己酮cyclohexanone√√???√甲乙酮methylethylketone√√●●?√异丙基丙酮isopropylacetone√√?√●○甲基异丁酮mibk√√?√?√乙酸乙酯ethylacetate√√√??√乙酸甲酯methylacetate●√●??√乙酸戊酯amylacetate√√√●?√乙酸丁酯butylacetate√√√●?√乙酸丙酯propylacetate●?√??√乙酸乙氧乙酯2-ethoxyethylacetate●●●●●√苯甲酸苄酯benzylbenzoate√√○√√√乙醚ethylether√√√●●√二氧六环dioxane√√●??●四氢呋喃tetrahydrofuran(thf)√√●??●二甲亚砜dmso●√√??●二甲基甲酰胺dimethylformamide(dmf)√√???●乙酰二乙胺diethylacetamide√√√??√三乙醇胺triethanolamine√√√√√√苯胺aniline●√√?●√吡啶pyridine√?●??√乙腈acetonitrile√√√??√10%苯酚phenolaqueous,10%?√●?●√30%甲醛formaldehydesolution,30%√√√●√●30%过氧化氢hydrogenperoxide,30%?√√√√√硅油siliconeoil√√√√√√√=推荐使用?=不推荐使用●=有限制性使用○=无应用说明

产品推荐

我们为你甄选择好产品