Basf巴斯夫 Flamestab NOR 116 FF

  • 产品品牌巴斯夫
  • 产品商标Flamestab
  • 产品型号NOR 116 FF
  • 产品规格
  • 产品产地德国
产品特性

It shows flame retardancy efficacy in polyolefin fibers, nonwovens and films at concentra - tions as low as 1%. Flamestab NOR 116 shows excellent polymer compat - ibility and high extraction resistance. It also provides superior light and ther - mal stability to the polymer and shows low interaction with acidic species deriving from pesticide residues or other halogenated products.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

产品英文名Flamestab NOR 116 FF

物理与规格

技术指标Melting Range 108 – 123 °C Specific gravity 1.06 g/ml Bulk density 0.28 g/ml Angle of repose 47 ° Flashpoint > 100 °C -4 Vapor Pressure (20 °C) 1.10 Pa Solubility (20 °C) % w/w Water <40 ppb Volatility (pure subsdtance; TGA, heating rate 20 °C/min in air) Weight Loss (%) Temperature °C 1.0 260 °C 10.0 285 °C
产品介绍

本产品为巴斯夫的Flamestab系列阻燃剂,型号NOR 116 FF,归入精细化学品与助剂 > 通用助剂 > 阻燃剂类别。品牌、商标、型号共同构成产品标识,便于采购核对与资料归档;该产品名称与分类信息可用于同类产品之间的区分。

应用场景

在下游配方与生产配料中可作为阻燃剂类原料使用,适配需要该类原料的体系。具体用法需结合下游工艺确定;并做好批次与工艺记录。