The surface aspect of extruded automotive profile and window channels is a key performance parameter. Class “A” automotive surface applications demand a very low level of particles that could cause visible surface imperfections leading to rejects or ‘scrap’. In response to this market requirement, Cabot has developed a family of SPHERON carbon blacks appropriately identified by the suffix “A” to address carbon black related extruded surface imperfections.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

化学品名Carbon black
产品英文名SPHERON SO(SPSO)
CAS号1333-86-4
分子式C
分子量12.011

物理与规格

外观Steel gray to black greasy feeling solid.
熔点/沸点熔点:greater than 3500 °C;沸点:>4000 °C
技术指标SPHERON SO-1A carbon black exhibits Test Formulation: 100 phr EPDM, 80 phr Paraffinic Oil, Sulfur cure vulcanization system rubber reinforcement and processing ® properties similar to those of ASTM SPHERON SO-1A ASTM N539 N539 carbon black, but imparts fewer Loading (phr) 142 142 visible imperfections on the surfaces PROCESSING PROPERTIES of extruded rubber parts. Mooney Viscosity ML (1+4) at 100°C, (M.U.) 66 67
产品介绍

本产品为Cabot卡博特的炭黑,型号SPHERON,归入行业通用材料与填料 > 通用颜料/填料 > 炭黑类别。品牌、型号共同构成产品标识,便于采购核对与资料归档;该产品名称与分类信息可用于同类产品之间的区分。

应用场景

在下游配方与生产配料中可作为炭黑类原料使用,适配需要该类原料的体系。具体用法需结合下游工艺确定;并做好批次与工艺记录。