Chemours科慕 Ti-Pure R-960

  • 产品品牌Chemours科慕
  • 产品商标Ti-Pure
  • 产品型号R-960
  • 产品规格
  • 产品产地美国
产品特性

Ti-Pure™ R-960 is a rutile titanium dioxide pigment Because of its outstanding exterior durability, Ti-Pure™ manufactured by the chloride process for use in R-960 is the pigment of choice for many critical coatings applications requiring outstanding chalk resistance, applications including: gloss retention, and tint retention.

应用

In addition to excellent • automotive OEM topcoat and refinish exterior durability, Ti-Pure™ R-960 provides very good • high durability exterior coil coatings dispersion with excellent hiding power and color acceptance. • aerospace coatings • powder coatings Table 1.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

化学品名Titanium dioxide
产品英文名Ti-Pure R-960
CAS号13463-67-7
分子式O2Ti
分子量79.866

物理与规格

外观White powder in two crystalline forms, anatase and rutile
熔点/沸点熔点:1855 °C;沸点:2500-3000 °C
产品介绍

本产品为Chemours科慕的Ti-Pure系列钛白粉,型号R-960,归入行业通用材料与填料 > 通用颜料/填料 > 钛白粉类别。品牌、商标、型号共同构成产品标识,便于采购核对与资料归档。

应用场景

在下游配方与生产配料中可作为钛白粉类原料使用,适配需要该类原料的体系。具体用法需结合下游工艺确定;并做好批次与工艺记录。