Dow陶氏 二丙二醇DPG(工业级)

  • 产品品牌Dow陶氏
  • 产品型号
  • 产品规格
  • 产品产地泰国
应用

Esterification with benzoic acid to make dipropylene glycol dibenzoate for plasticizers . 2. A reactant in unsaturated polyester resins to add flexibility and hydrolytic stability to the finished resin . 3. Esterification with acrylic acid to make dipropylene glycol diacrylate for radiation cured resin formulations . 4. In dicyclopentadiene - based unsaturated polyeste r resin systems to add flexibility . 5.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

化学品名1,1'-Oxydi-2-propanol
产品英文名DPG Dipropylene Glycol
CAS号110-98-5
分子式C6H14O3
分子量134.17

物理与规格

外观Colorless, slightly viscous liquid
熔点/沸点熔点:less than -40 °C;沸点:232.8 °C
纯度Dipropylene glycol regular grade is a distilled product of greater than 99% purity (as DPG), and is available from The Dow Chemical Company in drum and bulk quantities.
产品介绍

本产品为Dow陶氏的醇类,归入涂料、油墨及原材料 > 溶剂/稀释剂 > 醇类类别。品牌共同构成产品标识,便于采购核对与资料归档;该产品名称与分类信息可用于同类产品之间的区分。

应用场景

在下游配方与生产配料中可作为醇类类原料使用,适配需要该类原料的体系。具体用法需结合下游工艺确定;并做好批次与工艺记录。

产品推荐

我们为你甄选择好产品

企业动态

Enterprise dynamics