化学识别

化学品名Titanium dioxide
产品英文名TIOXIDE TR81
CAS号13463-67-7
分子式O2Ti
分子量79.866

物理与规格

外观White powder in two crystalline forms, anatase and rutile
熔点/沸点熔点:1855 °C;沸点:2500-3000 °C
包装规格Packaging Venator’s titanium dioxide pigments are available in 25kg bags and a range of flexible intermediate bulk containers. This communication is a general g
技术指标Inorganic coating Alumina, Zirconia Organic treatment Present Crystal size [μm] 0.25 3 Specific gravity [g/cm ] 4.1 (1) Loss at 105°C [%] 0.6 (2) 3 Bulk density (tamped) [g/cm ] 1.1 (3) 3 Oil absorption [cm /g pigment] 17/100 (4) 3 Water demand [cm /g pigment] 23/100 Durability Super durable ISO 591 classification R2 C.A.S No. 13463-67-7 (1) Measured within 48 hours of production. (2) Based on ISO 787/11. (3) Palette knife method, ISO 787/5. (4) In the presence of 0.4% sodium salt of complex polyphosphate calculated on the mass of pigment. This data sheet includes the
产品介绍

本品由Venator泛能拓出品,TIOXIDE系列型号TR81,属于行业通用材料与填料 > 通用颜料/填料 > 钛白粉类别。名称、品牌与分类信息完整,适合在采购目录和配方资料中归档。

应用场景

可用于钛白粉相关配方与生产环节,作为该类原料参与下游配料。具体用法需结合下游工艺与配方要求确定;并做好批次与工艺记录。

产品推荐

我们为你甄选择好产品

企业动态

Enterprise dynamics