White colloidal powder of high purity.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

化学品名Fumed silica
产品英文名HDK H 18
CAS号112945-52-5
分子式O2Si
分子量60.084

物理与规格

外观Amorphous powder
熔点/沸点熔点:1710 °C;沸点:2230 °C
包装规格160 kg (big bag on pallet)
技术指标Typical general characteristics Inspection Method Value SiO content (based on the substance heated at 1000 °C for 2 h) DIN EN ISO 3262 - 19 > 99,8 % ² Density at 20 °C (SiO ) - approx. 2,2 g/cm³ ² Residual silanol content 25 % (relative silanol content in relation to the hydrophilic silica, which shows approx. 2 SiOH/nm² ) 2 BET surface of the hydrophobic silica DIN ISO 9277 approx. 120 m /g DIN 66132 INCI name Silica Dimethyl Silylate Physical - chemical properties 2 BET surface of the hydrophilic silica DIN ISO 9277 170 - 230 m /g DIN 66132 Carbon content DIN ISO 10694 4,0 - 5,2 % pH - Value in 4 % dispersion (1 : 1 mixture of water - methanol) - 4,0 - 6,8 Tamped density DIN EN ISO 787 - 11 approx. 50 g/l Loss on drying , ex works (2 h at 105 °C) DIN EN ISO 787 - 2 < 0,6 % Sieve residue , acc. to Mocker > 40 μm DIN EN ISO 787 - 18 < 0,3 % Surface modification Polydimethylsiloxy These figures are only intended as a guide and should not be
产品介绍

本产品为Wacker瓦克旗下气相法二氧化硅产品,型号HDK H 18,归类于行业通用材料与填料 > 通用颜料/填料 > 气相法二氧化硅类别。产品以品牌、型号作为识别信息,便于采购与配方管理中的分类归档。

应用场景

可作为气相法二氧化硅类原料参与下游配方设计与生产配料,适合需要该类原料的体系。具体用法与工艺条件需结合下游配方确定。

产品推荐

我们为你甄选择好产品

企业动态

Enterprise dynamics