化学识别

化学品名Fumed silica
产品英文名HDK H 2000
CAS号112945-52-5
分子式O2Si
分子量60.084

物理与规格

外观Amorphous powder
熔点/沸点熔点:1710 °C;沸点:2230 °C
包装规格20 kg bags (320 kg per pallet)
技术指标Typcial general properties 1) SiO -content DIN 55921 % >99.8 2 Density of SiO g/l 2200 2 2 Silanol group density SiOH/nm < 0.5 13 Electrical resistivity (density 200 g/l) [ Ω cm] >10 Physical and chemical properties 2 BET-surface area of hydrophilic silica DIN 66131 m /g 170 - 230 2 BET-surface area DIN 66131 m /g 110 - 170 Carbon content % ca. 2.8 2) pH, in 4 % dispersion DIN ISO 787/9 6.5 – 8.0 Tamped density DIN ISO 787/11 g/l ca. 200 3) Loss on drying (2 h at 105°C) DIN ISO 787/2 % < 0.6 Surface modification -OSi(CH ) 3 3 1) Based on the substance heated at 1000 °C for 2 h 2) 1:1 mixture of water-methanol 3) Ex works These figures are intended as a guide and should not be
产品介绍

本产品为Wacker瓦克旗下气相法二氧化硅产品,型号HDK H 2000,归类于行业通用材料与填料 > 通用颜料/填料 > 气相法二氧化硅类别。产品以品牌、型号作为识别信息,便于采购与配方管理中的分类归档。

应用场景

可作为气相法二氧化硅类原料参与下游配方设计与生产配料,适合需要该类原料的体系。具体用法与工艺条件需结合下游配方确定。