欢迎来到凯茵化工国产品牌站
主图

Wacker瓦克 VINNOL E 15/45 M

  • 产品品牌Wacker瓦克
  • 产品商标VINNOL
  • 产品型号E 15/45 M
  • 产品规格
  • 产品产地德国
应用

Epoxy compounds often suffice to stabilize these coatings against low thermal impact.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

产品英文名VINNOL E 15/45 M

物理与规格

技术指标Specification Property Condition Value Method K- value - 44 - 46 DIN EN ISO 1628- 2 Viscosity, dynamic (20% in 20 °C 35 - 45 mPa·s DIN 53015 (20°C) MEK)⁽¹⁾ Acid number / saponification - 6 - 8 mg KOH/g specific method number Chlorine content - 47. 1 - 48. 3 wt. % specific method Volatiles - < 0. 5 wt. % specific method 1 after dissolving at 50 °C General Characteristics Property Condition Value Method Efflux time (20% in MEK) - approx. 34 s DIN EN ISO 2431 (4 mm) white granulate with some Supply form - Visual powder Bulk density - approx. 510 kg/m³ DIN EN ISO 60 Density - 1. 38 g/cm³ DIN 66137- 2 DSC (DIN 53765 / ISO Glass transition temperature - approx. 73 °C 11357- 5) Molecular weight (Mw) - 50000 - 60000 g/mol SEC, PS- Standard Particle size - < 2. 5 mm specific method These figures are only intended as a guide and should not be
产品介绍

作为Wacker瓦克的VINNOL系列氯醋树脂产品,本品型号E 15/45 M,在分类上属于涂料、油墨及原材料 > 树脂/乳液 > 氯醋树脂类别。产品信息以品牌与型号为主,便于分类管理;该产品名称与分类信息可用于同类产品之间的区分。

应用场景

适合作为氯醋树脂类原料进入下游配方体系,参与生产配料环节。具体用法与工艺条件需结合下游配方确定;并做好批次与工艺记录。

产品推荐

我们为你甄选择好产品

企业动态

Enterprise dynamics