欢迎来到凯茵化工国产品牌站
主图

Wacker瓦克 VINNOL E22/48A

  • 产品品牌Wacker瓦克
  • 产品商标VINNOL
  • 产品型号E22/48A
  • 产品规格
  • 产品产地德国
应用

Epoxy compounds often suffice to stabilize these coatings against low thermal impact.

咨询热线

咨询热线

扫码领试样

扫码领试样

化学识别

产品英文名VINNOL E22/48A

物理与规格

技术指标Specification Property Condition Value Method K- value - 47 - 49 DIN EN ISO 1628- 2 Viscosity, dynamic (20% in 20 °C 38 - 52 mPa·s DIN 53015 (20°C) MEK)⁽¹⁾ Chlorine content - 42. 0 - 43. 2 wt. % specific method Volatiles - < 0. 7 wt. % specific method 1 after dissolving at 50 °C General Characteristics Property Condition Value Method Efflux time (20% in MEK) - approx. 46 s DIN EN ISO 2431 (4 mm) white granulate with some Supply form - Visual powder DSC (DIN 53765 / ISO Glass transition temperature - approx. 61 °C 11357- 5) Molecular weight (Mw) - 60000 - 80000 g/mol SEC, PS- Standard Particle size - < 2. 5 mm specific method These figures are only intended as a guide and should not be
产品介绍

本品由Wacker瓦克出品,VINNOL系列型号E22/48A,属于涂料、油墨及原材料 > 树脂/乳液 > 氯醋树脂类别。名称、品牌与分类信息完整,适合在采购目录和配方资料中归档;该产品名称与分类信息可用于同类产品之间的区分。

应用场景

可用于氯醋树脂相关配方与生产环节,作为该类原料参与下游配料。具体用法需结合下游工艺与配方要求确定;并做好批次与工艺记录。

产品推荐

我们为你甄选择好产品

企业动态

Enterprise dynamics